Has anyone successfully dealt with this? One side of my hull is almost completely crazed, not stress cracking but crarzing like the gelcoat was too thick maybe. The cracks are completely over the topsides of the hull on only one side except on the flared portion of the bow (shaded?)
I don't want to peel it to glass just solvent wash, sand, and squeegy some epoxy over the whole thing b/4 epoxy primer and Perfection paint.
If no one has successfully done this, I am open to any and all suggestions as to epoxy brand or type. 1971 and white
I don't want to peel it to glass just solvent wash, sand, and squeegy some epoxy over the whole thing b/4 epoxy primer and Perfection paint.
If no one has successfully done this, I am open to any and all suggestions as to epoxy brand or type. 1971 and white