Reply
 
Thread Tools Search this Thread Display Modes
 
Old 05-03-2019, 10:59 AM   #1
Member
 
City: Portland
Join Date: Jun 2017
Posts: 13
Badly oxidized gel coat

Any suggestions on how to make an old boat that has been in the weather shine? The gel coat is oxidized and I am having a hard time figuring out what to use. The internet has a ton of products that all claim to do a great job.

Thanks!
Rhonda
High Fin is offline   Reply With Quote
Old 05-03-2019, 11:07 AM   #2
Guru
 
Martin J's Avatar
 
City: Mt Crested Butte
Vessel Name: Artemis
Vessel Model: Cheoy Lee 67
Join Date: Feb 2013
Posts: 551
If it's really bad use 3M super duty rubbing compound, and a 3M compounding pad, has to be done by machine. In my yards we used 3M products extensively and found this the best for heavy oxidized gel coat. You can follow up with a restorer/ wax after and then you'll be good for a few years, just by using restorer /wax on a annual basis.
Martin J is offline   Reply With Quote
Old 05-03-2019, 11:24 AM   #3
Senior Member
 
City: South Louisiana
Join Date: Oct 2017
Posts: 100
Quote:
Originally Posted by Martin J View Post
If it's really bad use 3M super duty rubbing compound, and a 3M compounding pad, has to be done by machine. In my yards we used 3M products extensively and found this the best for heavy oxidized gel coat. You can follow up with a restorer/ wax after and then you'll be good for a few years, just by using restorer /wax on a annual basis.
This is what I would do. It is a lot of work but very rewarding.
I have bought several boats that were very badly oxidized. I would compounded and waxed them when I got them home. It usually took a couple of weekends but they looked great when I finished. I would then use them for the summer and sell at the end of the summer for several thousand more than I bought them for.
latravcha is offline   Reply With Quote
Old 05-03-2019, 11:24 AM   #4
TF Site Team
 
Bacchus's Avatar
 
City: Seneca Lake NY
Vessel Name: Bacchus
Vessel Model: MS 34 HT Trawler
Join Date: Nov 2014
Posts: 7,826
If really bad it saves time to start w wet & dry sand paper using a block. 1200 if bad followed by 1600 - 2000 grit. Or go to the diner to start if not too bad. Then compound then swirl remover in steps. It will take some experimenting to determine how aggressive you need. Gosl should be to start with least aggressive starting step that doesn't take an excessive time to get improvement. How manyk steps depends on where you start. Using proper pads for cutting is also key.
Lots of help info & videos online.
There is no miracle one step product if badly oxidized.... IMO
__________________
Don
2008 MS 34 HT Trawler
"Bacchus"
Bacchus is online now   Reply With Quote
Old 05-03-2019, 11:32 AM   #5
Guru
 
Russell Clifton's Avatar
 
City: La Conner Wa.
Vessel Name: Sea Fever
Vessel Model: Defever 49 RPH
Join Date: Sep 2012
Posts: 877
You will definitely want to use a buffer. 3M makes excellent products. Like Martin J says rubbing compound if it's really, really bad. Or if it's just bad then a compounding product will work. The difference is how much grit they have in them. This will be a three step process. Step two would be to apply a polish. This will restore the shine. Step three is to apply wax, which will protect the polish. Do some research on the type of pad to use on the buffer for different products. If you use foam pads they will actually provide a little cut too. Different colors have different uses.

If you use a regular buffer you need to be extra careful about getting the surface to hot and burning it or actually removing excessive gel coat, especially on edges and corners. I use a Porter Cable random orbital buffer. Much more user friendly for the DIY.
Russell Clifton is offline   Reply With Quote
Old 05-03-2019, 12:06 PM   #6
Guru
 
AKDoug's Avatar
 
City: Kenai, Alaska
Vessel Name: Melanie Rose
Vessel Model: 1999 Willard PH
Join Date: Feb 2013
Posts: 1,236
Another vote for a good buffer and 3M, my boat was in that condition when I bought it, never waxed or buffed. It took one heavy pass of 3M Heavy cutting compound to reach the shine, and then another of 3M Finessit to really bring back the original color and shine. I bought a Makita buffer, where you can lock the trigger and vary the speed with the knob on the grip.

I wind up Finessing every other year and applying a coat (or two) of wax to make it shine. Mostly the buffing removes tar and rub marks from the fenders and dock after the first buffing.

It's a whole lot easier to do when it's on the hard, and you can stand in the back of your truck and drive around the outside of the boat buffing :-)
AKDoug is offline   Reply With Quote
Old 05-03-2019, 12:47 PM   #7
Senior Member
 
Sea Q's Avatar


 
City: Vancouver
Vessel Name: Sea Q
Vessel Model: Westport Mc Queen
Join Date: May 2015
Posts: 225
i would take a trip to Fishery Supplies and talk too the guys there.
They will not steer you wrong.
Sea Q is offline   Reply With Quote
Old 05-05-2019, 09:13 AM   #8
Senior Member
 
Puffin_NT32's Avatar
 
City: Watch Hill RI
Vessel Name: Puffin
Vessel Model: Nordic Tug 32/34
Join Date: Jan 2008
Posts: 172
My regimen for oxidized fiberglass is to wet sand with dual-action polisher, polish with 3M Finesse-It, then wax and buff. I use a Harbor Freight 6" DA polisher ($60), and have a 5" hook and loop pad. Use 5" 400, 1000, and 2000 grit hook and loop discs. Use a spray bottle with water and a little Dawn to keep the area wet while sanding. I use the DA polisher 6" foam pad to apply the Finesse-It, then buff it off with microfiber towels. I finish up with Collinite wax applied and buffed out with microfiber towels by hand. I prefer to wax and buff by hand because it leaves more wax on the surface than would a power buffing polisher.
Puffin_NT32 is offline   Reply With Quote
Old 05-05-2019, 10:06 AM   #9
TF Site Team
 
koliver's Avatar
 
City: Saltspring Island
Vessel Name: Retreat
Vessel Model: C&L 44
Join Date: Nov 2007
Posts: 5,663
Start with this: https://www.collinite.com/marine-wax...s-boat-cleaner
Wax with Collinite wax.
I have tried the others, including 3M Finessit. I find the Collinite is more aggressive, so get to the result faster.
__________________
Keith
koliver is offline   Reply With Quote
Old 05-05-2019, 10:51 AM   #10
Moderator Emeritus
 
Comodave's Avatar
 
City: Au Gres, MI
Vessel Name: Black Dog
Vessel Model: Formula 41PC
Join Date: Jul 2015
Posts: 21,185
Paint.
Comodave is offline   Reply With Quote
Old 05-05-2019, 10:53 AM   #11
Guru
 
psneeld's Avatar
 
City: Ft Pierce
Vessel Name: Sold
Vessel Model: Was an Albin/PSN 40
Join Date: Oct 2011
Posts: 28,145
If an older boat and badly oxidized, you may be better off letting a pro do it..... Unless you are very experienced.


I have seen wayyyyy too many gel coats ruined by going too far and now you either refel or paint. I did a lot through the years and still went through the gel on really bad boats and even some not so bad boats but ones that had thin gel.


Better someone else doing it than you. .. it's a tossup for sure.
psneeld is online now   Reply With Quote
Old 05-05-2019, 11:48 AM   #12
Guru
 
City: Anacortes
Join Date: Mar 2016
Posts: 588
Do all you can to try and save your gelcoat before considering paint. Gelcoat is more durable than even the best paints.
sean9c is offline   Reply With Quote
Old 05-05-2019, 02:53 PM   #13
Senior Member
 
Panacea123's Avatar
 
City: Cape Coral, Fl
Vessel Name: Panacea
Vessel Model: Novatec 42 Sundeck Trawler
Join Date: Jul 2016
Posts: 163
Some good advice here so far.
Have done it all including wet sand rubbing compound etc.
If it’s too far gone, Poly Glow is an excellent alternative.
Works as advertised look it up on Google.
In my experience it will degrade and yellow some after a while, but the good news is it washes right off with their Poly Prep or industrial wax stripper, then just apply another coating.
Panacea123 is offline   Reply With Quote
Old 05-05-2019, 03:01 PM   #14
Guru
 
City: Great Lakes
Vessel Model: OA 440
Join Date: Aug 2017
Posts: 904
I used 3M Imperial, which 3M says combines medium aggressive cutting with a polishing action....no swirls. It works! One step. Depends on just how bad the oxidation is on your boat, but I'd try a quart of Imperial before going to a heavy cutting compound and then having to do a second pass with something like Finesse it. I used the big, cheap variable speed polishers from Harbor Freight. Wore out the gears in one out about 3/4 through the job.. Still have the second one. But you need the variable speed feature. Think I used a white wool pad versus the yellow (whichever is the least aggressive of the two). There's a special tool to clean the dried compound out of the pad on occasion... a screw driver works, though. Hard on the arms and shoulders....
Rufus is offline   Reply With Quote
Old 05-06-2019, 06:17 AM   #15
FF
Guru
 
FF's Avatar
 
Join Date: Oct 2007
Posts: 22,553
"Gelcoat is more durable than even the best paints."

I am not so sure of that, many top yards seem to prefer paint on new GRP boats.

Marlow? Abeking & Rassmusen?
FF is offline   Reply With Quote
Old 05-06-2019, 09:17 AM   #16
Guru
 
Pau Hana's Avatar


 
City: Seattle, WA
Vessel Name: Pau Hana
Vessel Model: 1989 PT52 Overseas Yachtfisher
Join Date: Aug 2012
Posts: 2,676
Wrap it! We did so, and love the results!

https://www.boatus.com/magazine/2017...t-wrapping.asp
__________________
Peter- Marine Insurance Guru at Novamar Insurance Group (206-350-5051) & tuna fishing addict!

1989 52' PT Overseas yachtfisher
Pau Hana is offline   Reply With Quote
Old 05-06-2019, 10:03 AM   #17
TF Site Team
 
Larry M's Avatar
 
City: Jacksonville
Join Date: Nov 2008
Posts: 11,681
Peter:

What’s the expected life span? How are repairs made, if needed?
Larry M is online now   Reply With Quote
Old 05-06-2019, 10:09 AM   #18
Guru
 
Pau Hana's Avatar


 
City: Seattle, WA
Vessel Name: Pau Hana
Vessel Model: 1989 PT52 Overseas Yachtfisher
Join Date: Aug 2012
Posts: 2,676
Quote:
Originally Posted by Larry M View Post
Peter:

What’s the expected life span? How are repairs made, if needed?
Larry, the lifespan depends on location (sun exposure)- 3-5 years towards the tropics, and 8-10 years in northern climes like Seattle.

The film is a basecoat/clearcoat 3M product, so fade in minimal if at all. Simply cut out the damaged area, cut a new piece slightly larger than the cutout, clean the hull with alcohol, and apply the patch.
__________________
Peter- Marine Insurance Guru at Novamar Insurance Group (206-350-5051) & tuna fishing addict!

1989 52' PT Overseas yachtfisher
Pau Hana is offline   Reply With Quote
Old 05-06-2019, 11:11 AM   #19
Guru
 
Alaskan Sea-Duction's Avatar
 
City: Inside Passage Summer/Columbia River Winter
Vessel Name: Alaskan Sea-Duction
Vessel Model: 1988 M/Y Camargue YachtFisher
Join Date: Jul 2012
Posts: 8,050
Visit this website. I use the Dual Action Pro-polisher and some "Buff Magic." Talk to the folks at Shurhold. They are very happy to help you. They also have instructional videos. I use this stuff and found it to be awesome! I have no interest in Shurhold other than their stuff works.

https://shurhold.com/collections/dua...n-polisher-pro
Alaskan Sea-Duction is offline   Reply With Quote
Old 05-06-2019, 11:11 AM   #20
Guru
 
porman's Avatar
 
City: Duvall, Wa. USA
Vessel Name: Beach Music II
Vessel Model: 2003 Mainship 430 Trawler
Join Date: Aug 2014
Posts: 1,040
I've seen Peter's boat. The wrap looks terrific.
porman is offline   Reply With Quote
Reply

Thread Tools Search this Thread
Search this Thread:

Advanced Search
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off


» Trawler Port Captains
Port Captains are TF volunteers who can serve as local guides or assist with local arrangements and information. Search below to locate Port Captains near your destination. To learn more about this program read here: TF Port Captain Program





All times are GMT -5. The time now is 06:59 AM.


Powered by vBulletin® Version 3.8.8 Beta 4
Copyright ©2000 - 2024, vBulletin Solutions, Inc.
Search Engine Optimization by vBSEO 3.6.0
Copyright 2006 - 2012